Keletso | Yuniti | GM30 | GM31 | Ym40 | ||||
Botenya | μm | 50 | 125 | 50 | 125 | 50 | 125 | |
Matla a tšepe | MD | Mpa | 215 | 180 | 196 | 201 | 221 | 224 |
TD | Mpa | 252 | 210 | 231 | 215 | 234 | 242 | |
Emplation | MD | % | 145 | 135 | 142 | 161 | 165 | 146 |
TD | % | 108 | 135 | 120 | 127 | 128 | 132 | |
Shrinkage (150 ℃ / 30min) | MD | % | 0.7 | 0.5 | 0.5 | 1.1 | 1.2 | 1.2 |
TD | % | 0.2 | 0.2 | 0.4 | 0.9 | 0.04 | 0.01 | |
Transmittance | % | 90.2 | 90.3 | 90.2 | 90.1 | 90.2 | 90.3 | |
Haze | % | 1.6 | 1.8 | 2.4 | 3.4 | 2.02 | 2.68 | |
Ho hlaka | % | 99.4 | 99.3 | 97.6 | 94.6 | - | - |